Thus, PS films that were too thick (filmsthicker than 0.2% PS with plasma treatment shorter than 60 s, or PS films fabricated with higher PS concentrations than 0.4% plasma
treated for 0–150 s), were not capable of improving the protein binding signals in
immunoassay, and only ultrathin PS films could significantly improve the protein bioassay performance