TS1 composite produced by hydrolysis of TiCl4 solution exhibited
higher TiO2 content (37 wt.%) than that of TS2 composite
(20 wt.%) produced by TiO2 suspension. However, TiO2 in the
TS1 nanocomposite revealed larger grain size compared with the
TiO2 in the TS2 composite.