using a drop coating technique, 20 L of a colloidal suspension of the AuNPs was added to the surface of the electrode followed by drying at room temperature. To obtain a similar electroactive surface area on both types of electrodes, several drops of colloidal suspension were added to the electrode, and the optimal volume of AuNPs was determined to be 20 L.