The tensile strength actually increased from 3 to 8 MPa as a result of ultrasonication at 28 kHz. To improve and stabilize the dispersion state, five kinds of dispersant were used.
The tensile strength actually increased from 3 to 8 MPa as a result of ultrasonicationat 28 kHz. To improve and stabilize the dispersion state, five kinds of dispersant were used.