Fig. 5 (right) shows the AIε values for the same samples; the main observation is that the samples treated at 30 RPM are rigid compared to the more elastic samples obtained at 20 RPM.
Fig. 5 (right) shows the AIε values for the same samples; the mainobservation is that the samples treated at 30 RPM are rigidcompared to the more elastic samples obtained at 20 RPM.