The testing procedure followed here differs from that used by other authors since a galvanostatic and not a potentiostatic method of current application was used. Galvanostatic control enables a careful monitoring of constant corrosion rates throughout the test, while potentiostatic tests suppose a variation of the dissolution rate (current recorded) over the testing time.