To provide Web Nano fibers Chitosan/PVA, a solvent with a density of 2.7% weight by volume, and the ratio (75:25) provided in solvent acetic acid and water were mixed, then, the resulting solvent was stirred for 12 h at the temperature of the room, next, the obtained solvent was electrospinned which was done under the processing condition voltage 18 kV, feeding rate 0.35 ml/h and the distance from collector to tip is 15 cm.