This observation was further supported by the XRD result.
In addition to this shell layer, interplanar lattice spacing of 0.35
nm corresponding to the (101) plane of anatase phase of TiO2
were also observed in the core region, which suggested that the
TNFs in the composite were in the anatase phase.