The Pt NPs were deposited into TiO2 film at -445 mV (versus SCE) inan aqueous solution of 5 mM K2PtCl4+ 0.1 M K2SO4 with the magnetic stirring. Finally, the electrode was rinsed with pure water anddried for surface characterization and electrochemical study.