The influence of sample cutting on the residual stresses
obtained by means of a XRD analysis is studied in this part.
A strain gauge is glued in the drilled hole to record strains
during sample cutting and to compare strains before and after
cutting. The strains are measured in three directions 0°, 45°
and 90°. 45° corresponds to circumferential direction