Accordingly to prepare PPy/Fe3O4 nanocomposites,0.4 g of Fe3O4 was added to 80 mL deionised water in a conical flask and ultra-sonicated for 10 min for better dispersion of
Fe3O4 in water.6 g of FeCl 3 (oxidant) was added into the deionised
water containing Fe3O4