The
maximum strain was not severely affected by the low percentages
(0.5e1%) of unmodified lignin, mainly in the case of organosolv
lignin. However, at percentages greater than 5%, the maximum
strain decreased with increasing lignin content, especially in blends
formed by PLA and commercial lignin.