As the acrylate rubber content increased up to 10%, a weak and broad crystallization peak upon first heating appeared with a peak temperature around 112 ◦C.
As the acrylate rubber content increased up to 10%, a weak and broad crystallizationpeak upon first heating appeared with a peak temperature around 112 ◦C.