The addition of the natural plasticizer to the film shifted the Tg shift towards lower temperatures, from 63.6 C in the latex film to 67.7 C in the plasticized latex film. Similar Tg values are found in the literature for natural rubber latex
The addition of the natural plasticizerto the film shifted the Tg shift towards lowertemperatures, from 63.6 C in the latex film to 67.7 C inthe plasticized latex film. Similar Tg values are found in theliterature for natural rubber latex