. Positive electrode laminates (LFP, LMO and LCO)
were prepared by mixing 84 wt% active electrode materials, 8 wt%
acetylene black and 8 wt% poly(vinylidene difluoride) (PVDF) in 1-
methyl-2-pyrrolidinone (NMP) into slurries and then casting them
on an aluminum foil.