On a glass of the project present along the line,
the surface preparation has to be done as per IO SS by the personnel in charge.
The structural sealing shall be applied, using the template,
in vertical position (on the glass in the metal rack).
After 24h a peeling test has to be done in order to verify the correct adhesion of the sealing and the integrity of the finish. The result has been recorded on the QCR 30.2 V by the line foreman.
After the test, the glass has to be re-used in production.