The spectra for chitosan-based films dried at room temperature were similar, regardless of glycerol amount. It is noteworthy that films had excellent barrier properties to light in the UV region, being the preventive effect slightly better for LMw chitosan-based films. when films were heat-treated, there was a sharp increase in absorbance in the range of 200–400 nm for higher glycerol contents.