After that, the mixed powders were filtered and dried at 80 oC. The molding process of PES/PTFE Blends was as follows: the mixed powders were pressed at room temperature with a pressure of 40 MPa for 10 min.
After that, the mixed powders were filtered and dried at80 oC. The molding process of PES/PTFE Blends was asfollows: the mixed powders were pressed at room temperaturewith a pressure of 40 MPa for 10 min.