The horn tacked on over the lessons was used to keep the lessons from being soiled by the child. The horn of oxen and sheep were used to make the laminating structure. The horn was left in cold water for several weeks, which separated the usable part from the bone. It was then heated, first in boiling water then by fire, and pressed by plates and machines to make it smooth and transparent.