3. Maintain minimal printing unit pressure. Capsule
rupture due to high printing pressures causes the
blanket and sometimes the plate to become oil
covered. If enough oil is transferred to the plate, the
non-image area of the plate may become ink receptive.
In addition, the blanket and plate may also turn
the color of the capsule dyes. Recommended printing
nip squeeze is 0.003 to 0.005 inches.