The experimental evolution of the elastic (G0) and viscous (G00) modules, and the tangent of the phase angle (tand) for PP,
HDPE and LDPE at 180 C without UV irradiation and for chosen frequency 10 rad s1 are illustrated at Fig. 2. The data were
extracted from multiwave experiment.