The measured values from the pick-up coil are evaluated on the
complex impedance plane. An important parameter is the frequency
of the excited alternating current. Due to the skin effect, the
depth of excitation in the specimen decreases with increasing frequency.
The point where the eddy current density has decreased to
1/e, or approximately 37% of the surface density, is called the
standard depth of penetration d