Nuts retained on the 14 mm sieve, which was most abundant in the samples were used to eliminate variation with nut size. Each experimental value is an average of 15 replicates, loading one nut at a time until it fails. Samples of nuts retained on other sieve sizes were loaded to failure to facilitate a comparison of observed cracking force for different nut grades with estimates from other experiments.