The CdS QDs were deposited by CBD method. The CBD process involved dipping the ZnO nanorods in the aqueous solution consisting of 0.1 M Na2S for 5min and then in 0.1M CdCl2 for 5min at the room temperature. The two-step dipping procedure was considered one CBD cycle.