For TGA measurement, approximately 8 mg of the silica/NR masterbatch
sample was heated from 40 C to 600 C at
a heating rate of 20 C/min under nitrogen atmosphere.
Then, the gas was automatically changed to oxygen and the
sample was continuously heated up to 800 C.