The raw material, with particle size between 250 and 425 mm,
was placed in a horizontal stainless steel reactor and heated in a
furnace at the rate of 20 8C min1 from room temperature to
500 8C, and maintained at this temperature for 2 h under N2 flow of
100 cm3 min1 for obtaining of carbonized material (Cb).