The obtained ZnO/TiO2 nanocomposite rods were
annealed at 500 C and 600 C. ZnO/TiO2 nanocomposite rods have
been characterized by X-ray Diffraction (XRD) for average crystallite
size and phase of the composite material, Particle Size Analyser
(PSA) for average particle size, Scanning Electron Microscope (SEM)
and Transmission Electron Microscope (TEM) for morphology
study, Energy Dispersive X-ray Spectrometry (EDX) for elemental
analysis, and Thermal Gravimetric and Differential Thermal Analysis
(TG–DTA) for thermal property.