The samples showing the highest amount of particle deposits
is the reference pellets, especially in position “A” (Figure 8),
where the intensity of the substrate, Fe, Cr and Ni was low.
From the SEM analysis it seems that there are fewer deposits
for the pellet with additives compared to the reference pellet.