which was found only 30% reduction at 4.0 wt.% blowing agent addition because the decomposition of the blowing agent was not suitable for the melting temperature of the PP matrix
which was found only 30% reduction at4.0 wt.% blowing agent addition because the decomposition ofthe blowing agent was not suitable for the melting temperature of the PP matrix