However, the
present investigation revealed that the compressive strength of
concrete specimens developed using GRP waste powder was found
to be higher than that of the normal requirement for precast
concrete walling element (>5 MPa), lightweight concrete(>5 MPa), and concrete blocks (7–35 MPa) and confirmed the
potential applications of GRP waste as an additive or filler in
concrete.