Crack growth is monitored using a magnifying lens and the measurements of the load and displacement at the corresponding crack length are recorded. Moreover, the fracture surfaces of the specimens are examined by SEM (Zeiss LEO982 operating at 1 kV) with and without solvent etching (THF, Biosolve) of the phenoxy phase. Images are captured from 100× to 30,000× magnification