The precipitates were filtered, washed with distilled water until free from chloride ions (checked by AgNO3 solution). The catalyst was dried in an oven at a temperature of 110 C for 12 h and treated with H2SO4 (1 N, 15 ml/g) for 30 min followed by calcination at 600 C for 4 h.