From TEM observation, 2000 kDa PS has the most smooth nanofibers due to its enough long molecular chains (Fig. 1a), 200 kDa PS has ultrafine nanofibers with some nodes (Fig. 1b), whereas 20 kDa PS produces flower-like nanofibers due to its short chains (Fig. 1c).