The purpose of this test is to understand what happens to the finished tablet after it adsorbs and desorbs moisture many times. The question is: Does the finished tablet lose performance after adsorbing and desorbing moisture many times? The current test will help answer this question. Maybe it will show it’s a significant issue, or maybe it will show that it is not a significant issue. No additional testing is needed right now, but let’s discuss the results when they are complete.
Overall, the main focus should continue to be the performance loss during the manufacturing process. We still don’t fully understand why the performance decreases during the process. There is still a big opportunity to identify the cause and find a solution to this problem.
Below is a summary of the in-process tests and some open questions (items 4,5,& 6) that will soon need investigation. There is some evidence to support these (4,5 & 6) variables are important. Since items (1,2 & 3) are already in-process, would you like to get started on 4,5 & 6?
Also, would you like to create the trial plan for each item, or do you want to work together on setting up the trials? Either way is OK.