Also two MA modified EPM rubbers (0.7 wt% MA) were used, both having a relatively low
molecular weight. The two modified EPM rubbers differ in the ethylene-propylene ratio; 75/25 and
50/50 wt%. These rubbers were kindly supplied by Exxon Chemical, trade name Exxelor.