preparation of catalyst by dry impregnation after Calcinations support at temperature 550 2 hr to get rid of the impurities mixed in a solution of sodium carbonate 45% dry at temperature 120 16 hr the Calcinations temperature 550 5 hr the catalyst received to keep it in Disiccator before the test reaction