Sharp large peaks are visible from 3000 to 3600 cm−1, which indicates OH stretching. In the untreated and PAA-pretreated SWBC, these peaks were centered at 3348 cm−1 but in the PAA + IL pretreated samples, the peak centers shift to higher bands. This indicates that a weakening of the hydrogen bonds occurred in the cellulose structure