Due to the very slow crystallization kinetics of this grade of PLA
[18], the injection-moulded samples resulted to be fully amorphous.
These samples will be referred to as amorphous PLA. In
order to obtain fully crystalline samples, some moulded samples
were kept in an oven at 105 C (namely the temperature of maximum
crystallization rate for this material) for 8 h.