Sampleswere pre-conditioned (finalmoisture level: 40 g/100 g) before HP treatments. Both the HP treated
and the untreated rawmaterialswere evaluated for pasting properties and solvent retention capacity, and investigated
by differential scanning calorimetry, X-ray diffractometry and environmental scanning electron
microscopy