At 800 oC, there is generally complete loss of water in OPC concrete, which has a significant impact on the compressive strength of the sample. Because of this phase change, the residual strength of OPC concrete dropped from 51% to a very low of 21%. Both the geopolymer concretes showed similar (27–29%) residual strengths at this temperature range.