-The IP and team were not following ATH Tack Welding Procedure. Tack welds should have been minimum 50mm and on both sides of the strong back. The preparation for the welds had also not been carried out resulting in lack of fusion between strong back and deck.-Using a sledgehammer when a smaller heavy hammer should have been used.