For class II composite restorations, choosing composites with a low shrinkage value and
elastic modulus, applying an incremental filling technique of more than three layers, and
polymerizing them with sufficient curing time are needed to reduce the cuspal deflection,
which is induced by the polymerization shrinkage stress of composites.