According to some previous studies from the literature on activated carbon production by H3PO4 and ZnCl2 activation, the optimal activation conditions were: the weight ratio of the activation agent to precursor of 1–2, activation/carbonization temperature of 400–500°C and activation time of 0.5–2 h [6,8,9].