describes the overall synthesis process of PACS. During
the heat-treatment process, petroleum asphalt melts and
uniformly envelops ZnO templates with thin carbon layer before
condensation. Afterwards, the mixture is carbonized at 1073 K
for 1 h. With the assistance of nitric acid solution, the metal oxide