The prepared IUCPE was anodized by successive cyclic voltammetry for 35 cycles from −0.30V to +1.50V with a scan rate of 100 mV/s in NaOH (0.20 mol/L). After the pre-anodization, the electrode was thoroughly rinsed with double distilled deionized water and dried in the air.