differences, both polymers show complete decomposition above
500 1C. Accordingly, the firing of the ceramic bodies included a
short dwell stage (15 min) at 500 1C to allow polymer decomposition. The absence of polymeric residues or ashes in the
sintered discs indicates that these polymers can be used as poreforming agents.