Temperature had only a marginal impact on the capacity decay in this set of experiments. The OCVs before charging at 0 C were 25e30 mV larger than those at 20 C. The reason for this observation was that during the pervious discharge process,the battery operating at lower temperature terminated earlier as discussed above, and hence more capacity remained in the electrolytes instead of being discharged.