The accumulation potential and time were set at, −200 mV and 300 s, respectively, and the scan rate at 50 mV s−1 in the scan range of −200 to 700 mV. The resulting electrode demonstrated a linear response over range of silver ion concentration of 8.0–80 pmol/L with detection limit (S/N = 3) of 5 pmol/L