This work aims to produce geopolymer mixed water ,Portland cement and granulated blast-furnace slag (GBFS) By sodium hydroxide (SH) in the form of a solid to dissolve in water and added to calcium carbonate (CC) then dried at 80 °C for 8 hr followed by pulverization to a fixed particle size to produce the dry activator consisting of calcium hydroxide, sodium carbonate and pirssonite