In the
case of mesoporous pure TiO2 film (sample A), 60% of the MB
dye still remained after 60 min.In contrast, mesoporous TiO2/
SiO2 hybrid films displayed much faster photodegradation.
When the amount of SiO2 was increased, the photodegradation
activity was also dramatically increased